Why Do Carbon Fiber Modulus and Strength Numbers Vary So Much? And Which Should You Design With?
You’re sizing a motor-mount bracket for a multi-rotor UAV arm. The fiber datasheet lists 700 KSI as the tensile strength. A laminate table for the same fiber lists the tensile strength as a fraction of that. Both are correct, but they describe different things, and you need to know which one belongs in your design calculations.
This article explains what each value describes and which one to design with.
Three levels, three different numbers
Two of the most commonly requested properties of a carbon fiber laminate are tensile strength and modulus. The values of those properties depend on what is being described.
Fiber properties. These are the stiffness and strength properties of the carbon fiber itself, taken from a datasheet for a specific fiber. These are typically the highest numbers you will see. Commonly used standard modulus fibers often have a tensile strength of around 700 KSI and a modulus of around 33 MSI.
Composite laminate properties. Laminates are composed of fibers aligned in multiple orientations in multiple layers, and bound together by a cured resin. The stiffness and strength of a laminate come from the fibers and are higher along fiber axes. Strength and stiffness values are calculated over a cross-sectional area (lbs per square inch). A laminate has lower properties than the fiber alone due to the percentage of resin and non-axis fibers contained within that cross-sectional area.
For example, a 0/90 standard modulus carbon fiber laminate composed of 700 KSI tensile strength fibers will typically have a tensile strength in the range of 80 to 100 KSI. The same laminate has a tensile modulus (stiffness) near 5 to 10 MSI, less than a third of the fiber’s roughly 33 MSI modulus.
Geometry, loading and boundary conditions. The geometry, loading, and boundary conditions of a part affect local stresses, as well as part strength and deflection under load. For example, a plate and a tube can have the same laminate design and moduli, but will have significantly different deflections under a bending load.
Fiber classes: Strength vs. stiffness
Carbon fiber is produced in four modulus classes. Typical fiber-level values:
Fiber class | Fiber modulus (MSI, fiber-level) |
Standard modulus | ~33 to 35 |
Intermediate modulus | ~40 to 47 |
High modulus | ~50 to 65 |
Ultra-high modulus | ~75 to 135 |
Ultra-high modulus fibers have lower tensile strengths and are more brittle than the lower modulus fibers. Account for this when designing with them. Ultra-high modulus fiber is roughly three times as stiff as standard modulus, which makes it worth the added cost where deflection, dimensional stability or natural frequency drive the design. However, when strength or damage tolerance are more important, standard, intermediate, or high modulus are usually a better choice.
Factors affecting composite properties
The modulus and tensile strength of a composite laminate are determined by several factors. The table below lists the most common factors and how each one affects modulus and tensile strength.
Factor | Effect on the modulus of a laminate | Effect on tensile strength of a laminate |
Fiber choice | Primary driver of modulus | Primary driver of tensile strength |
Resin choice | Affects load transfer between fibers and deflection of a part | Affects load transfer between fibers and strength of a part |
Manufacturing method | Higher-temperature cures produce stiffer resins and laminates | Voids and fiber distortion reduce strength more than stiffness. Different manufacturing methods result in different fiber content and voids as well as the degree of fiber distortion. |
Fiber orientation | Modulus in a specific direction depends on the amount of fiber running in that direction | Same dependence. Off-axis loading results in lower strength |
Part shape | Section shape affects deflection | Holes, notches and corners create stress concentrations and can cause the composite to crack locally |
Loading and boundary conditions | Details of part constraint and loading affect deflection | A laminate will fail very differently in tension, compression, bending or impact |
Account for all of these factors when designing a carbon fiber part.
Other materials vary with direction too, to a lesser degree
Design tables treat 6061 aluminum as isotropic, yet the properties of extruded aluminum vary with direction. Wood is more anisotropic than aluminum: strength along the grain is much higher than strength across the grain, and builders of boats and wooden aircraft have to account for how properties change with the axis being loaded.
Application to the design process
- Start with recommended design properties. For a 0/90 layup, Element 6 provides conservative design properties, for example about 90 KSI ultimate tensile. The maximum theoretical values are greater than that number, but the recommended design properties account for the variables described above.
- Finite element analysis (FEA) provides higher resolution: expected deflection and local stress levels. Element 6 offers finite element analysis as a paid service.
- Refine the design. During the analysis phase, different fibers and orientations can be evaluated. For part features that may cause stress concentrations, localized reinforcements can be evaluated.
- Verify by test. Material properties and analyses should be validated by physical testing for your specific application.
Element 6 engineers can walk you through the material properties for your application. Talk to Our Engineers
Frequently asked questions
Why does carbon fiber have so many different strength values? Published values are measured at different levels: a single fiber, a flat laminate or a finished part. Every level adds complexity: fiber and resin selection, fiber orientation, geometry, loading and boundary conditions. Do not use fiber values as laminate properties in the design process.
Which carbon fiber number should I use to design a part? Start with a conservative design number for your layup, then refine with FEA and testing. Fiber datasheet values describe the fiber alone, not the final part.